1.配料:先按比例秤好夜光粉(含量约占2~10%),加入小量的扩散油(石蜡油、白扩油)搅拌成糊状,再加进原料搅拌,再加色粉搅拌,搅拌均匀,时间不宜太长避免夜光粉沉淀,注意夜光粉*忌跟铁等重金属磨擦,会使原料变黑。可以使用的材质有:PP,PE,PVC,PU,PS,ABS,TPR,EVA,PMMA,尼龙等。塑胶材质越透明,发光效果越好,色粉尽量用荧光色粉,添加越少越好。
2.注塑:注塑机温度调到低,可注塑即可,料在注塑机内时间不宜太长,以免烧焦。
3.注塑机:不同机器注塑出的产品,也有区别,新机器与旧机器,国产机器与进口机器,这都需要慢慢调试中解决。
4.夜光粉:长效夜光粉在注塑方面由于各种原因,注塑技术、注塑机器,都可能引起发黑,可根据自己的情况实验确定。
1.Ingredients: initially the proportional scales well luminous powder (content of
Plus stir into the raw materials, coupled with the toner stirring, stir, time not too long to avoid luminous powder precipitated Note luminous powder with iron and other heavy very sensitive
Metal friction, make raw black. Material: PP, PE, PVC, PU, PS, ABS, TPR, EVA, PMMA, such as nylon.
The plastic material is more transparent, glow, toner try using fluorescent toner, add as little as possible.
2. Injection: injection molding machine temperature to the minimum can be injection molded to material in the injection molding machine time not too long, to avoid burning.
3. Injection molding machine: different machine injection molding products, the difference between the new machine and the old machine, domestic machines and
Debugging resolved.
4. Luminous powder: long-lasting glow powder injection molding for various reasons, injection technology, injection molding machines, are likely to cause black, according to their own
The case is determined experimentally.
The information from Yao Desheng Ke technology: http://yeguangcailiao.com please indicate!